Ingredients: 3 gr kaolin clay 0,50 gr zinc oxide 0,40 gr arrowroot powder 1 ml Alcohol 2, 5 gr Dryed pigment 0,05 ml Sharomix 705

Process: 1. In a mortar add the kaolin clay, zinc oxide, and arrowroot powder with Dried pigment 2. Grind everything carefully until you have a homogeneous color and everything looks united. 3. When the entire mixture is uniform in color add the alcohol and the sharomix 705. 6. Pour everything into an aluminum mold and use parchment paper and press to make it quite compact. let it dry overnight before using

Properties: Transparency: X Opacity: Elasticity: Smell: Flexibility: Stamina: Mustiness:

X X X X XXXX X